Difference between revisions of "Upgrade/RFFoil/WoodsMetal"

From LHCb Wiki
Jump to navigation Jump to search
Line 28: Line 28:
  
 
Cerrolow 136 (58 �C) is about half the price of Field's metal (62 �C). What do we need to look at:
 
Cerrolow 136 (58 �C) is about half the price of Field's metal (62 �C). What do we need to look at:
  - difference in melting temperature relevant? (how warm could foil become while machining?)
+
* difference in melting temperature relevant? (how warm could foil become while machining?)
  - difference in toxity: Field's metal does not contain lead and less bismuth
+
* difference in toxity: Field's metal does not contain lead and less bismuth
  - Al affinity: how easy can we get it off?
+
* Al affinity: how easy can we get it off?
  - recoverability: stuff is rather expensive (count 20k Euro for final box). how well can we recover it?
+
* recoverability: stuff is rather expensive (count 20k Euro for final box). how well can we recover it?